view the rest of the comments
3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io
There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)
Moderation policy: Light, mostly invisible
I use multiple materials from multiple brands, so yes, I do some calibration for each filaments.
I usually limit myself to the flow factor by printing a cube in vase mode and then adjust by ±2% after a print if I feel like it is needed.
For the temperatures, I go for the normal recommended values (200°C hot end and 60°C bed for PLA) without any calibration, unless there is a problem. (I think last time I printed one was for ABS because it kept curling up..)
Retraction and Linear advance seems to always give roughly the same value for each type of materials, so I ended up using an average which work well enough.
I now feel like an idiot that I’ve never thought of turning on vase mode for a calibration cube