When I do an overhang test, I always have this problem at about 35°. Does anyone have a suggestion what could be causing it?

  • Slicer: Orca
  • Layer height: 0.2mm
  • Infill: 0% (this has improved it a lot, I think the infill was causing bulging)
  • Outer walls: 2
  • Overhang speed: 10 or 20mm/s (both look the same)

Solution: I mistakenly thought overhang speed in Orca was based on overhang angle, it is percentage instead (which makes much more sense for different layer heights). My 10-25% overhang speed wasn't set to slow down and that must translate to about 35° at 0.2mm layer height. I now have it set to 30mm/s and it now looks great 👍 And sorry, I was wrong when I stated the overhang speed 😅

top 16 comments
sorted by: hot top controversial new old
[-] MotoAsh@lemmy.world 9 points 7 months ago

The corners are slowly curling up more and more until the nozzle goes completely outside of the curl and becomes an overhanged corner.

The biggest problem is what ever is causing your plastic to curl while printing. Some plastics are terrible for it and you basically need a heated chamber to get rid of it. You could try playing with cooling settings or making a warmer environment, or ... something else. Half the time if it's a problem, I have to change the print or its orientation or add geometry so it doesn't curl... It's such a pain sometimes.

[-] UnH1ng3d@lemmy.world 3 points 7 months ago

Thanks. I'll experiment with temperatures first but I've got some different filament on the way too as it happens, so hopefully I'll manage to escape the problem one way or another 😁

[-] rambos@lemm.ee 1 points 7 months ago

I thought curling as well, but I would expect that on higher angles instead. Its easy to confirm this if you watch the print. The solution would be lowering nozzle temp and slowing down the print (well, not less than 10 mm/s). I've seen that also too much cooling can cause curling, but thats for super strong part cooling

[-] themoonisacheese@sh.itjust.works 6 points 7 months ago

Seems like lowering your hot end temps or increasing cooling would do the trick

[-] Valmond@lemmy.world 6 points 7 months ago

I came here to say augment the print temperature! Look at those non binding "tubes" that are laid down every layer! They should melt into each other or it's just crap and they'll break under their own weight.

Upping the fan is not needed here (yet, see below). It's good when doing overhangs or printing without support and stuff start to sag down. When anything sags down probably :-)

So up the temp for the overhangs, if they become too "liquid" then up the cooling(so fan speed).

[-] UnH1ng3d@lemmy.world 3 points 7 months ago

Thanks guys. I will try both and see what works. My layer adhesion is good / parts are strong though.

[-] JoShmoe@ani.social 3 points 7 months ago

Looks like the deformation is happening on the same layers where the overhangs of the number 35 are.

[-] UnH1ng3d@lemmy.world 3 points 7 months ago

It starts just underneath actually, but it still could be related 🤔 Maybe I need a test without numbers.

[-] damium@programming.dev 4 points 7 months ago

If 35° (or something close to it) is the slicer setting for overhang detection it likely changes the cooling/speed/flow settings. If that is the case you can set it to a lower detection value and maybe get better results or change the normal cooling/speed/flow to be closer so it isn't as drastic of a change.

[-] UnH1ng3d@lemmy.world 2 points 7 months ago

You may actually be right even though I thought I had checked this. Orca's overhang speeds are based on overhang percentage and not angle, I previously just looked at the number and assumed it was degrees 🤦‍♂️I will match the speeds for all overhang percentage ranges and see if that solves it 🤞

[-] UnH1ng3d@lemmy.world 1 points 7 months ago

This was it! I had my 10-25% (not degrees 😅) overhang speed set not to slow down at all. I now have it set to 30mm/s and I have a perfect result. Thank you 👍😁

[-] JoShmoe@ani.social 1 points 7 months ago

I believe that if your layers are printing fast enough, the softer material would bend according to where the top layer is printed.

[-] UnH1ng3d@lemmy.world 1 points 7 months ago

Sorry, I didn't follow that. Top layer of what? Not the actual top, top layer right?

[-] JoShmoe@ani.social 2 points 7 months ago

I meant, the next layer directly on top of where your deformed layers begin.

[-] HeyLow 3 points 7 months ago

Looks like drooping to me, I would see if lowering nozzle temp improves/solves this

[-] UnH1ng3d@lemmy.world 1 points 7 months ago

Thanks, I'll give it a go.

this post was submitted on 12 Apr 2024
42 points (100.0% liked)

3DPrinting

15577 readers
48 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS