19

You can see where around corners and even some straight runs it is peeling up. I'm running first layer at an agonizing 15 mm/s. Using hatchbox pla filament, just dried in dehydrator. 200° nozzle and 70° bed. The glass is freshly cleaned with soap and water, I just did several atomic pulls, I've trammed at different heights using a feeler gauge, and absolutely nothing is working. Any one have any ideas?

you are viewing a single comment's thread
view the rest of the comments
[-] Grass@sh.itjust.works 1 points 5 months ago* (last edited 5 months ago)

Those lines dont look flat enough to me. https://ellis3dp.com/Print-Tuning-Guide/articles/first_layer_squish.html

The guide is largely klipper oriented but has marlin instructions after the klipper instructions.

Other than that I've tried some samples of bed adhesion aid of different brands which help for printing some of the bullshit filaments that stick to literally nothing and they are much less messy than hairspray or glue and most didn't smell awful, but I haven't found them to actually be necessary for anything other than the really slippery filaments.

this post was submitted on 12 Jan 2024
19 points (100.0% liked)

3D Printing

4296 readers
1 users here now

For everyhting 3D printing related.

Please be excellent to each other :)

Icon by Freepik, Banner photo by Thiago Medeiros Araujo

founded 3 years ago
MODERATORS