127

This is PETG, one was left out in about 40% humidity the other was dried to about 20%

you are viewing a single comment's thread
view the rest of the comments
[-] OR3X@lemmy.world 7 points 1 week ago

Weird. I've never dried my filament and never have this issue.

[-] the16bitgamer@programming.dev 5 points 1 week ago

It's PETG and I've moved to a very wet environment. Stringing and popping and a big issue here. My last place though was a lot dryer and didn't need this solution.

[-] clb92@feddit.dk 3 points 1 week ago

It also depends how humid it is where you live.

[-] Sxan@piefed.zip 1 points 1 week ago

Maybe it has someþing to do wiþ þe fact þat you live in Death Valley

this post was submitted on 17 Aug 2025
127 points (100.0% liked)

3DPrinting

19520 readers
217 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS