view the rest of the comments
Ask Lemmy
A Fediverse community for open-ended, thought provoking questions
Rules: (interactive)
1) Be nice and; have fun
Doxxing, trolling, sealioning, racism, and toxicity are not welcomed in AskLemmy. Remember what your mother said: if you can't say something nice, don't say anything at all. In addition, the site-wide Lemmy.world terms of service also apply here. Please familiarize yourself with them
2) All posts must end with a '?'
This is sort of like Jeopardy. Please phrase all post titles in the form of a proper question ending with ?
3) No spam
Please do not flood the community with nonsense. Actual suspected spammers will be banned on site. No astroturfing.
4) NSFW is okay, within reason
Just remember to tag posts with either a content warning or a [NSFW] tag. Overtly sexual posts are not allowed, please direct them to either !asklemmyafterdark@lemmy.world or !asklemmynsfw@lemmynsfw.com.
NSFW comments should be restricted to posts tagged [NSFW].
5) This is not a support community.
It is not a place for 'how do I?', type questions.
If you have any questions regarding the site itself or would like to report a community, please direct them to Lemmy.world Support or email info@lemmy.world. For other questions check our partnered communities list, or use the search function.
6) No US Politics.
Please don't post about current US Politics. If you need to do this, try !politicaldiscussion@lemmy.world or !askusa@discuss.online
Reminder: The terms of service apply here too.
Partnered Communities:
Logo design credit goes to: tubbadu
PETG just is a pain in the ass sometimes. Really sensitive to moisture, and it loves to stick to hot metal. So it has a tendency to overextrude because of the steam, and bunch up on the nozzle, causing all sorts of havok.
The key to printing it is just keeping it dry -- the latest batches I've held feel like they're way softer than I remember, so I suspect mfgs are putting more glycol in it than before.
Also, do a sanity check and go back and print PLA from time to time. Sometimes you won't realize something else is wrong and you'll blame it on the filament, but something like the idler arm on the extruder is broken, etc.
You can print it on Textured PEI, or Glass - but I suggest putting a little glue stick down to act as a release agent on the PEI - PETG and PEI bond together too well in some instances (ESPECIALLY on smooth PEI)