Im impressed. It's fibron. I'll order some salt and let it hang out in its naked glory.

[-] Therustynut@forum.guncadindex.com 1 points 1 day ago* (last edited 23 hours ago)

flower salt not sure of what that is,? I was going too anneal in the air firer, same one for drying PA.

Edit, is there a need too add moisture into the print afterwards? Im still a bit new to PACF

ok, did some reading. so can i get away with a dish of regular table salt. then 100c for a whopping 16 hrs? damn.

4
"law tactical" style AR adapter. (forum.guncadindex.com)

Has anyone tried a law tactical style adapter? Pretty sure it couldn't be made all that sturdy considering the stresses on the component. I'm making a sl9 and was tempted too make it as short as possible.

7
annealing PA612CF (forum.guncadindex.com)

I have a hoffman sl9 running in the bambu as I type. Whats some preferred tips and tricks for annealing. Ive heard the obvious temp and time. Do I leave the supports on while its cooking? thanks.