7
annealing PA612CF
(forum.guncadindex.com)
Post here if you have general questions concerning GunCAD, printing, or otherwise fabricating DIY firearms. Newbies are welcome, but users are encouraged to read Ctrl+PEW's Getting Started Guide if they haven't already.
Shitty stock image may be changed at moderator discretion.
flower salt not sure of what that is,? I was going too anneal in the air firer, same one for drying PA.
Edit, is there a need too add moisture into the print afterwards? Im still a bit new to PACF
ok, did some reading. so can i get away with a dish of regular table salt. then 100c for a whopping 16 hrs? damn.